摘要

PURPOSE: A barium aluminate-based fluorescent material and its preparation method are provided, which is improved in the luminous brightness under UV and VUV (vacuum UV) and is suitable for a lamp and PDP. CONSTITUTION: The barium aluminate-based fluorescent material is represented by the formula 1, wherein 0.5x1.5, 0y0.4, and 0z0.4. The color of the barium aluminate-based fluorescent material is blue when 0.5x1.5, y=0, and 0.02z0.4, and green when 0.5x1.5, 0.05y0.4, and z=0, or when 0.5x1.5, 0.005y0.4, and 0.05z 0.4. The method comprises the steps of dissolving the precursors of a fluorescent material, an activating material and a lubricant to make a precursor solution; and sintering the precursor solution under the reductive condition of hydrogen gas at 1,200-1,400 deg.C. Preferably the precursors are Ba(NO3)2, Al(NO3)3, Mn(NO3)2 and Eu(NO3)3.
机译:目的:提供一种基于铝酸钡的荧光材料及其制备方法,其在UV和VUV(真空UV)下的发光亮度得到改善,并且适用于灯和PDP。组成:铝酸钡基荧光材料由式1表示,其中0.5x1.5、0y0.4和0z0.4。铝酸钡基荧光材料的颜色在0.5x1.5,y = 0和0.02z0.4时为蓝色,在0.5x1.5、0.05y0.4和z = 0或0.5x1时为绿色。 .5、0.005y0.4和0.05z 0.4。该方法包括以下步骤:溶解荧光材料,活化材料和润滑剂的前体以制备前体溶液;然后将前体溶液溶解。在氢气的还原条件下,在1200〜1400℃下烧结前体溶液。优选地,前体是Ba(NO 3)2,Al(NO 3)3,Mn(NO 3)2和Eu(NO 3)3。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号