Highly crater-resistant high-strength sintered material.

机译:高度抗缩孔的高强度烧结材料。

摘要

A sintered material containing high-pressure phase-type boron nitride and a binder is provided. The high-pressure phase-type boron nitride is contained in an amount of from 50% to 78% by volume, and the balance is a binder phase. The binder phase comprises at least one selected from the group consisting of nitride, carbide, carbonitride, and boride of Ti, nitride, boride and oxide of Al, carbide and boride of W, nitride, carbide, carbonitride and boride of Co, and carbide and boride of Ni, or a mutual solid solution thereof. The binder phase forms a binder phase which is continuous in a sintered material texture. The weight of metal components Al, W, Co and Ni which are present as compounds in the sintered material is from 3% to 20% based on the sintered material. The sintered material is excellent in crater resistance and capable of realizing a long tool life, even under the condition that the temperature of the cutting edge becomes high and the impact is large, as in high-speed interrupted cutting of hardened steel where the cutting speed V becomes at least 150 m/min. IMAGE
机译:提供包含高压相型氮化硼和粘合剂的烧结材料。高压相型氮化硼的含量为50体积%至78体积%,其余为粘合剂相。粘合剂相包括选自由以下组成的组中的至少一种:Ti的氮化物,碳化物,碳氮化物和硼化物,Al的氮化物,硼化物和氧化物,W的碳化物和硼化物,Co的氮化物,碳化物,碳氮化物和硼化物以及碳化物。 Ni的硼化物或其互固溶体。粘结剂相形成在烧结的材料织构中连续的粘结剂相。以化合物形式存在于烧结材料中的金属成分Al,W,Co和Ni的重量为烧结材料的3%至20%。该烧结材料即使在切削刃温度升高且冲击较大的情况下,也具有耐月牙洼的性能,并且能够实现较长的工具寿命,例如在高速间断切削淬硬钢的情况下,切削速度V至少达到150 m / min。 <图像>

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号