PURPOSE: Textile for an uncovered air bag is characterized by using low shrinkage polyamide fiber having 3-6% of dry heat shrinkage(160deg.C, 30min.) and having excellent tensile strength and tear strength. CONSTITUTION: Textile for an uncovered air bag is obtained by the steps of: (A) weaving grey textile out of low shrinkage polyamide fiber having 3-6% of dry heat shrinkage(160deg.C, 30min.); (B) passing continuously the grey textile in 3-10 of aqueous baths elevated gradually temperature by 5-20deg.C to heat-shrink; (C) passing the grey textile through a steam heating device to heat-shrink additively; and then (D) passing the textile through a hot blast drying device to dry. The textile has 200-300kg of tensile strength, 25-40kg of tear strength and under 1.0cm¬3/cm¬2/sec of air permeability.
机译:用途:一种用于未覆盖气囊的纺织品,其特征在于使用具有3-6%的干热收缩率(160℃,30分钟)且具有出色的拉伸强度和撕裂强度的低收缩聚酰胺纤维。组成:用于未覆盖安全气囊的纺织品是通过以下步骤获得的:(A)用干热收缩率为3-6%(160℃,30分钟)的低收缩聚酰胺纤维织成灰色纺织品; (B)使灰色纺织品在3-10℃的水浴中连续通过,使温度逐渐升高5-20℃以热收缩; (C)使坯布通过蒸汽加热装置以加热收缩;然后(D)使纺织品通过热风干燥装置进行干燥。该纺织品具有200-300kg的抗张强度,25-40kg的撕裂强度以及在1.0cm 3 / cm 2 /秒以下的透气率。

著录项

  • 公开/公告号KR100451262B1

    专利类型

  • 公开/公告日2004-09-22

    原文格式PDF

  • 申请/专利权人 HYOSUNG CORPORATION;

    申请/专利号KR20030073664

  • 发明设计人 LEE CHANG WHAN;YU JAE AN;

    申请日2003-10-22

  • 分类号D06C7/00;

  • 国家 KR

  • 入库时间 2022-08-21 22:46:38

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号