首页> 外国专利> Process for the oxygen delignification of pulp in two stages with higher pressure in the second stage

Process for the oxygen delignification of pulp in two stages with higher pressure in the second stage

机译:在第二阶段中以较高的压力分两个阶段对纸浆进行氧气脱木质素的过程

摘要

A system and process for the oxygen delignification of pulp consisting of a lignocellulose-containing material that has a mean concentration of 8-18% pulp consistency. The oxygen delignification takes place in a first stage with a short dwell time of about 3-6 minutes, at a low temperature of about 85° C. and under a low pressure of approximately 0-4 bar. A concluding stage has a longer dwell time of about 50-90 minutes, at a higher temperature of approximately 100° C. and under a higher pressure of about 8-10 bar.
机译:一种用于纸浆的氧气脱木素的系统和方法,该系统和方法由平均浓度为8-18%的纸浆浓度的含木质纤维素材料组成。氧脱木质素在第一阶段中以约3-6分钟的短停留时间在约85℃的低温和约0-4bar的低压下进行。最后阶段在约100℃的较高温度和约8-10bar的较高压力下具有约50-90分钟的较长停留时间。

著录项

  • 公开/公告号US6841036B2

    专利类型

  • 公开/公告日2005-01-11

    原文格式PDF

  • 申请/专利权人 HAKAN DAHLLOF;MARTIN RAGNAR;

    申请/专利号US20020121170

  • 发明设计人 HAKAN DAHLLOF;MARTIN RAGNAR;

    申请日2002-04-11

  • 分类号D21C9147;

  • 国家 US