首页> 外国专利> Production manner of the gear material for high-speed dry cutting and production mannered null mass of the gear which uses its

Production manner of the gear material for high-speed dry cutting and production mannered null mass of the gear which uses its

机译:用于高速干切削的齿轮材料的生产方式和使用其的齿轮的经生产的零质量

摘要

PROBLEM TO BE SOLVED: To provide a method for producing a blank for gear capable of securing the service life of a tool without any problems to be mass-produced even in the case of cutting the gear at the high speed of ≥200 m/min by dry-cutting without using a coolant, and to provide a method for producing the gear using this blank.;SOLUTION: The blank for forging, composed of a hot-rolled steel material containing by mass% of 0.15-0.30% C, ≤0.5% Si, 0.20-1.50% Mn, ≤0.03% P, ≤0.035% S, 0.30-2.00% Cr, 0.010-0.060% Al, 0.0080-0.0250% N, ≤0.015% O and if necessary, containing further, Mo and Ca and the balance Fe with inevitable impurities, is heated to 1,100-1,350°C and hot-forged and thereafter, a bainite transformation is completed during cooling and successively, heated and held to 620-750°C for 20 min-3 hr. A gear-cutting tool is desirable to use a cemented-carbide K sort alloy.;COPYRIGHT: (C)2006,JPO&NCIPI
机译:要解决的问题:提供一种用于制造齿轮坯料的方法,该方法即使在以200 m / ge的高速切削齿轮的情况下也能够确保工具的使用寿命而不会大量生产任何问题。 ;不使用冷却剂的情况下,通过干法切削最小分钟,并提供一种使用该坯料生产齿轮的方法。;解决方案:锻造坯料由质量百分比为0.15-0.30%C的热轧钢材组成, ≥0.5%Si,0.20-1.50%Mn,≤0.03%P,≥0.035%S,0.30-2.00%Cr,0.010-0.060%Al,0.0080-0.0250%N,≥0.015%O将其中进一步含有Mo和Ca以及余量为Fe且具有不可避免的杂质的余量的Fe加热到1,100-1,350℃并进行热锻,然后在冷却过程中完成贝氏体转变,并依次加热并保持在620-750℃持续20分钟至3小时。使用硬质合金K类合金是一种理想的齿轮切削工具。;版权所有:(C)2006,JPO&NCIPI

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号