首页> 外国专利> (1) precious metal content is 0.001 - 0.03 in the precious metal content compound

(1) precious metal content is 0.001 - 0.03 in the precious metal content compound

机译:(1)贵金属含量化合物中的贵金属含量为0.001-0.03%

摘要

PROBLEM TO BE SOLVED: To provide complex metal oxide containing an exhaust gas purification catalyst noble metal excellent in heat resistance of the whole pore volume and its manufacturing method.;SOLUTION: The complex metal oxide containing noble metals consisting of zirconium, cerium and noble metal has a whole pore volume after sintering at 1,050°C for 24 hours of 0.25 cc/g or more. It is preferable that the peak is pore diameter of 50-90 nm in micro pore profile based on BJH method, that the whole pore volume is 0.6 cc/g or more.;COPYRIGHT: (C)2006,JPO&NCIPI
机译:解决的问题:提供一种在排气孔净化催化剂中贵金属的整体孔体积的耐热性优异的复合金属氧化物及其制造方法。解决方法:含有锆,铈和贵金属构成的贵金属的复合金属氧化物在1050℃下烧结24小时后的总孔体积为0.25cc / g或更高。以BJH法为基准,在微孔分布中,峰优选为50-90nm的孔径,总孔体积为0.6cc / g以上。版权所有:(C)2006,JPO&NCIPI

著录项

  • 公开/公告号JP4450763B2

    专利类型

  • 公开/公告日2010-04-14

    原文格式PDF

  • 申请/专利权人 第一稀元素化学工業株式会社;

    申请/专利号JP20050112733

  • 发明设计人 近藤 大智;柳下 定寛;

    申请日2005-03-10

  • 分类号B01J23/63;B01D53/94;B01J35/10;B01J37/03;

  • 国家 JP

  • 入库时间 2022-08-21 18:58:26