Disclosed is a low-melting glass which has excellent water resistance and can impart excellent flame retardancy to a resin composition.  Also disclosed is a resin composition comprising the low-melting glass.  Further disclosed is a resin molded article.Specifically disclosed is a low-melting glass which comprises 22-27 mol% of P2O5, 3-18 mol% of SO3, 25-40 mol% of ZnO, 0-2 mol% of Al2O3, 0-4 mol% of Li2O, 0-15 mol% of Na2O and 11-35 mol% of K2O, wherein the total amount of Li2O, Na2O and K2O is 25-35 mol%.  The low-melting glass has a glass transition temperature of 200 to 300°C exclusive.  A resin composition is produced by mixing the low-melting glass with a resin.  A resin molded article is produced by molding or curing the resin composition.
机译:本发明公开了一种低熔点玻璃,其具有优异的耐水性并且可以赋予树脂组合物优异的阻燃性。还公开了包含低熔点玻璃的树脂组合物。还公开了一种树脂模制品。具体公开了一种低熔点玻璃,其包含22-27摩尔%的P 2 O 5,3-18摩尔%的SO 3,25-40摩尔%的ZnO,0-2摩尔%的Al 2 O 3,0-4摩尔%的Li 2 O, 0-15mol%的Na 2 O和11-35mol%的K 2 O,其中Li 2 O,Na 2 O和K 2 O的总量为25-35mol%。低熔点玻璃的玻璃化转变温度仅为200至300°C。通过将低熔点玻璃与树脂混合来制造树脂组合物。通过模制或固化树脂组合物来生产树脂模制品。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号