首页> 外国专利> ANODE ACTIVE MATERIAL OF THE NUCLEAR SHELL TYPE FOR LITHIUM SECONDARY BATTERIES, METHOD FOR PREPARING THIS MATERIAL AND LITHIUM SECONDARY BATTERIES CONTAINING THIS MATERIAL

ANODE ACTIVE MATERIAL OF THE NUCLEAR SHELL TYPE FOR LITHIUM SECONDARY BATTERIES, METHOD FOR PREPARING THIS MATERIAL AND LITHIUM SECONDARY BATTERIES CONTAINING THIS MATERIAL

机译:用于锂二次电池的核壳型阳极活性材料,该材料的制备方法以及包含该材料的锂二次电池

摘要

1. Anode active material of a nuclear-shell type for lithium secondary batteries containing a core of carbon-containing material and a shell molded on top of the core of carbon-containing material, the shell contains a material with PTC (positive temperature coefficient). ! 2. Anode active material of a nuclear-shell type for lithium secondary batteries according to claim 1, characterized in that the carbon-containing material of the core is at least one selected from the group consisting of soft carbon, hard carbon, natural graphite, quiche -graphite, pyrolytic carbon, carbon fibers based on mesophase pitch, mesocarbon beads, mesophase pitch, and petroleum and coal coke. ! 3. Anode active material of a nuclear-shell type for lithium secondary batteries according to claim 1, characterized in that the particles of the material with PTC have an average size of from 2 nm to 1 μm. ! 4. The anode active material of a nuclear-shell type for lithium secondary batteries according to claim 1, characterized in that the weight ratio of carbon-containing material and material with PTC is from 100: 0.1 to 100: 2. ! 5. Anode active material of a nuclear-shell type for lithium secondary batteries according to claim 1, characterized in that the material with PTC is barium titanate. ! 6. Anode active material of a nuclear-shell type for lithium secondary batteries according to claim 1, characterized in that the shell further comprises at least one metal oxide selected from the group consisting of titanium dioxide and spinel-type lithium oxide. ! 7. Anode active material of nuclear
机译:1.用于锂二次电池的核壳型阳极活性材料,其包含含碳材料的芯和模制在含碳材料的芯的顶部的壳,所述壳包含具有PTC(正温度系数)的材料。 ! 2.根据权利要求1所述的用于锂二次电池的核壳型阳极活性材料,其特征在于,所述核的含碳材料是选自由软碳,硬碳,天然石墨,乳蛋饼-石墨,热解碳,基于中间相沥青的碳纤维,中间相碳珠,中间相沥青以及石油和煤焦。 ! 3.根据权利要求1所述的用于锂二次电池的核壳型负极活性材料,其特征在于,所述具有PTC的材料的颗粒的平均尺寸为2nm至1μm。 ! 4.根据权利要求1所述的核二次电池用核壳型负极活性物质,其特征在于,所述含碳材料与具有PTC的材料的重量比为100∶0.1〜100∶2。 5.根据权利要求1的用于锂二次电池的核壳型阳极活性材料,其特征在于,带有PTC的材料是钛酸钡。 ! 6.根据权利要求1所述的核二次电池用核壳型负极活性物质,其特征在于,所述壳还包含选自二氧化钛和尖晶石型氧化锂中的至少一种金属氧化物。 ! 7.阳极核活性物质

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号