首页> 外国专利> METHOD OF PREPARING POSITIVE ACTIVE MATERIAL FOR RECHARGEABLE LITHIUM BATTERY USING IRON(III) OXIDE, POSITIVE ACTIVE MATERIAL FOR RECHARGEABLE LITHIUM BATTERY PREPARED BY USING THE METHOD, AND RECHARGEABLE LITHIUM BATTERY INCLUDING THE SAME

METHOD OF PREPARING POSITIVE ACTIVE MATERIAL FOR RECHARGEABLE LITHIUM BATTERY USING IRON(III) OXIDE, POSITIVE ACTIVE MATERIAL FOR RECHARGEABLE LITHIUM BATTERY PREPARED BY USING THE METHOD, AND RECHARGEABLE LITHIUM BATTERY INCLUDING THE SAME

机译:使用氧化铁(III)制备可充电锂电池的正极活性物质的方法,使用该方法制备的可充电锂电池的正极活性物质以及包括该锂离子电池的可充电锂电池

摘要

PURPOSE: A manufacturing method of anodic active material for lithium secondary battery using iron(III) oxide, anodic active material for the lithium secondary battery manufactured according to the manufacturing method, and a lithium secondary battery including thereof are provided to enhance profitability by using iron(III) oxide originated from waste iron, simplify manufacturing process, and solve waste resources transaction problem. CONSTITUTION: A manufacturing method of anodic active material for a lithium secondary battery comprises the following steps: forming trivalent iron ion by dissolving iron(III) oxide(Fe2O3) using a dissolution agent; forming divalent iron ion after reducing the trivalent iron ion as a reducing agent; forming precipitation by mixing the divalent iron ion, lithium source, phosphoric acid supply source, and solvent; and heat-treating the precipitation. The iron(III) oxide is originated from waste iron. The dissolution agent comprises acid, chelating agent, a combination thereof.
机译:目的:提供一种使用氧化铁(III)的锂二次电池用阳极活性材料的制造方法,根据该制造方法制造的锂二次电池用阳极活性材料以及包括其的锂二次电池,以通过使用铁来提高获利能力。 (三)源自废铁的氧化物,简化了生产工艺,解决了废料交易难题。组成:一种锂二次电池用阳极活性材料的制造方法,包括以下步骤:通过使用溶解剂溶解氧化铁(Fe2O3)形成三价铁离子;将三价铁离子还原为还原剂后形成二价铁离子。通过混合二价铁离子,锂源,磷酸供应源和溶剂形成沉淀。对沉淀物进行热处理。氧化铁(III)源自废铁。溶解剂包括酸,螯合剂,其组合。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号