The ferritic stainless steel null C which is superior in thermal fatigue property, fatigue at elevated temperature property

机译:热疲劳性,高温疲劳性优异的铁素体系不锈钢零碳

摘要

PROBLEM TO BE SOLVED: To provide a ferritic stainless steel which is excellent in thermal fatigue properties, high temperature fatigue properties and oxidation resistance, without using Mo and W and without causing deterioration in oxidation resistance due to addition of Cu.;SOLUTION: The ferritic stainless steel comprises, by mass%, ≤0.015% C, ≤1.0% Si, ≤0.5% Mn, ≤0.040% P, ≤0.010% S, ≤0.1% Al, 16 to 20% Cr, 0.8 to 1.6% Cu, 0.015 to 0.040% N, 0.15 to 0.60% V, Nb: 10×(C+N) to 0.60%, ≤0.01% Ti, ≤0.01% Zr, ≤0.01% Ta, ≤0.4% Ni, ≤0.1% Mo and ≤0.1% W, wherein the product of the V content and the N content satisfies (V×N): 0.003 to 0.015, and the balance Fe with inevitable impurities.;COPYRIGHT: (C)2010,JPO&INPIT
机译:要解决的问题:提供一种具有优异的热疲劳性能,高温疲劳性能和抗氧化性的铁素体不锈钢,而无需使用Mo和W,并且不会因添加Cu而导致抗氧化性下降;解决方案:铁素体以质量%计,不锈钢包括0.015%的C,1.0%的Si,0.5%的Mn,0.040%的P,0.010%的S,0.1%的Al,16%至20%的Cr,铜0.8至1.6%,氮0.015至0.040%,钒0.15至0.60%,Nb:10倍(C + N)至0.60%,钛0.01%,钛0.01%Zr,钛0.01%钽,钛; 0.4%Ni,0.1%Mo和0.1%W,其中V含量和N含量的乘积满足(V×N):0.003至0.015,其余的Fe带有不可避免的杂质。 (C)2010,日本特许厅&INPIT

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号