Methods for drawing gel-spun polyethylene yarns and stretch

机译:凝胶纺聚乙烯丝的拉伸和拉伸方法

摘要

A polyethylene multi-filament yarn is provided, which comprises a polyethylene having an intrinsic viscosity in decalin at 135°C of from 5 dl/g to 35 dl/g, fewer than two methyl groups per thousand carbon atoms, and less than 2 wt. % of other constituents. The yarn has a tenacity of at least 17 g/d as measured by ASTM D2256-02. The filaments of the yarn have a peak value of the ordered-sequence length distribution function, F(L), as determined at 23°C from the low frequency Raman band associated with the longitudinal acoustic mode (LAM-1), at a straight chain segment length L of at least 40 nanometers.
机译:提供了一种聚乙烯复丝纱线,其包含在135℃下萘烷中的特性粘度为5dl / g至35dl / g,每千个碳原子少于两个甲基且少于2wt%的聚乙烯。 。其他成分的百分比。根据ASTM D2256-02测量,该纱线的强度至少为17g / d。纱线的细丝在直线上具有23℃下从与纵向声模(LAM-1)相关的低频拉曼带所确定的有序序列长度分布函数F(L)的峰值。链段的长度L至少为40纳米。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号