This invention relates to a process which produces flat, distortion-free, zero-shrink, low-temperature co-fired ceramic (LTCC) bodies, composites, modules or packages from precursor green (unfired) laminates of three or more different dielectric tape chemistries that are configured in an uniquely or pseudo-symmetrical arrangement in the z-axis of the laminate.
机译:本发明涉及一种由三种或更多种不同的介电带化学物质的前体生坯(未烧制)层压板生产扁平,无变形,零收缩,低温共烧陶瓷(LTCC)体,复合材料,组件或包装的方法。在层压板的z轴上以唯一或伪对称的方式配置的组件。