首页> 外国专利> APPLICATION METHOD OF CORROSION PROTECTION COATING ONTO METAL PRODUCTS BY THERMODIFFUSION ZINC PLATING

APPLICATION METHOD OF CORROSION PROTECTION COATING ONTO METAL PRODUCTS BY THERMODIFFUSION ZINC PLATING

机译:热扩散锌镀层在金属制品上的防腐涂层应用方法

摘要

FIELD: metallurgy.;SUBSTANCE: corrosion protection coating is applied onto metal products in a sealed container arranged in a muffle furnace. Treated parts are arranged in the container in a regular manner in accessories with supporting surfaces, which fix them and prevent their direct contact between each other and movement relative to each other at movement of the container so that minimum distance between treated surfaces of parts is 3-5 mm. During zinc plating process, treated parts can perform movements relative to supporting surfaces of the accessories in the container by not more than 5-10 mm. Saturating mixture contains zinc crystals with purity of 0.97-0.99% of needle shape with coefficient of effective surface area of 10. Saturating mixture has particle size distribution at the interval of 3-7 mcm, and its weight is 1-4% of the weight of treated parts or 130-140% of the weight of the required coating on surface of treated parts.;EFFECT: increasing service life of a product owing to excluding its corrosion and increasing productivity of a furnace, in which diffusion zinc plating is performed; reducing zinc consumption in terms of per unit of surface of treated part.
机译:领域:冶金;物质:在马弗炉中布置的密封容器中,将腐蚀防护涂层涂覆到金属产品上。处理过的零件以规则的方式安排在带有支撑表面的附件中,该附件固定支撑并防止它们在容器运动时彼此直接接触以及彼此相对运动,因此零件的处理过的表面之间的最小距离为3 -5毫米在镀锌过程中,处理过的零件可相对于容器中附件的支撑面执行不超过5-10毫米的移动。饱和混合物包含纯度为针形的0.97-0.99%的锌晶体,有效表面积系数为10。饱和混合物的粒度分布在3-7 mcm的范围内,其重量为重量的1-4%。效果:由于排除了产品的腐蚀并提高了进行扩散镀锌的炉子的生产率,从而延长了产品的使用寿命,从而延长了产品的使用寿命;以被处理零件的单位面积减少锌的消耗量。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号