A preparation method for moisture-curing polyurethane reactive hot melt adhesive for textile composition mainly comprises the following steps: (1) mixing and stirring polyether polyol 4000E, polyester polyol 3000H, polyester polyol 2000N, and an antioxidant, heating the mixture to about 120℃, and then performing water removal for 0.5h under the condition that the vacuum degree is lower than 100 Pa; (2) adding a tackifying resin, heating the mixture to 135℃ to 140℃, and performing water removal under the condition that the vacuum degree is lower than 100 Pa; (3) lowering the temperature to 87℃, adding 4,4'-MDI, performing catalysis, stirring the mixture, and making the mixture react for 2h under the condition that the vacuum degree is lower than 100 Pa; (4) releasing vacuum, adding white carbon black, rapidly stirring the mixture evenly, and continuing to stir for 10 min under the condition that the vacuum degree is lower than 100 Pa; and (5) rapidly discharging at the kept temperature of 85℃ to 100℃, packaging, and then curing for 4h at 80℃ to 85℃, to obtain a target product. The product is used for textile composition, and has high peeling strength, a short opening time, desirable hydrolysis resistance performance, and high storage stability.
机译:一种用于纺织品组合物的湿气固化型聚氨酯反应性热熔胶的制备方法,主要包括以下步骤:(1)将聚醚多元醇4000E,聚酯多元醇3000H,聚酯多元醇2000N和抗氧化剂混合并搅拌,加热至约120℃。 ,然后在真空度低于100Pa的条件下进行0.5h的除水; (2)添加增粘树脂,将混合物加热至135℃至140℃,并在真空度低于100Pa的条件下进行除水; (3)在真空度低于100Pa的条件下,将温度降至87℃,加入4,4'-MDI,进行催化,搅拌混合物,使混合物反应2h。 (4)释放真空,加入白炭黑,迅速搅拌均匀,在真空度低于100Pa的条件下继续搅拌10分钟; (5)在85℃至100℃的温度下快速放电,包装,然后在80℃至85℃固化4h,得到目标产物。该产品用于纺织品组合物,具有高剥离强度,短打开时间,所需的耐水解性能和高储存稳定性。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号