A preparation method for moisture-curing polyurethane reactive hot melt adhesive for textile lamination mainly includes the following steps: (1) mixing and stirring polyether polyol 4000E, polyester polyol 3000H, polyester polyol 2000N, and an antioxidant, heating the mixture to about 120° C., and dehydrating for 0.5h under a vacuum of lower than 100 Pa; (2) adding a tackifying resin, heating the mixture to 135-140° C., and dehydrating for 1.5h under a vacuum of lower than 100 Pa; (3) lowering the temperature to 87° C., adding 4,4′-diphenylmethane diisocyanate and a catalysis, stirring the mixture, and reacting for 2h under a vacuum of lower than 100 Pa; (4) releasing vacuum, adding white carbon black, rapidly stirring the mixture evenly, and further stirring for 10 min under a vacuum of lower than 100 Pa; and (5) rapidly discharging at a temperature of 85-100° C., packaging, and then curing for 4h at 80-85° C., to obtain a target product. When applied in textile lamination, the product exhibits excellent peel strength, a relatively short open time, good hydrolysis resistance and desirable storage stability.
机译:用于织物层压的湿固化聚氨酯反应性热熔胶的制备方法主要包括以下步骤:(1)将聚醚多元醇4000E,聚酯多元醇3000H,聚酯多元醇2000N和抗氧化剂混合并搅拌,将混合物加热至约120°。并在低于100 Pa的真空下脱水0.5小时; (2)加入增粘树脂,加热至135-140℃,在低于100Pa的真空下脱水1.5h; (3)将温度降至87℃,加入4,4'-二苯基甲烷二异氰酸酯并进行催化,搅拌混合物,并在低于100Pa的真空下反应2h; (4)解除真空,加入白炭黑,迅速搅拌均匀,在低于100Pa的真空下再搅拌10分钟; (5)在85-100℃的温度下快速放电,包装,然后在80-85℃下固化4h,得到目标产物。当用于纺织品层压时,该产品表现出优异的剥离强度,相对短的开放时间,良好的耐水解性和所需的储存稳定性。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号