首页> 外国专利> Modified polyphenylene ether, a manufacturing method thereof, polyphenylene ether resin composition, a resin varnish, a prepreg, metal clad laminated board and printed wiring board

Modified polyphenylene ether, a manufacturing method thereof, polyphenylene ether resin composition, a resin varnish, a prepreg, metal clad laminated board and printed wiring board

机译:改性聚苯醚,其制造方法,聚苯醚树脂组合物,树脂清漆,半固化片,覆金属层压板和印刷线路板

摘要

A modified polyphenylene ether according to one aspect of the invention has an intrinsic viscosity, as measured in 25° C. methylene chloride, of from 0.03 to 0.12 dL/g, has on molecular ends thereof an average of 1.5 to 3 groups represented by formula (1) below per molecule, and includes not more than 5 mass % of a high-molecular-weight component having a molecular weight of 13,000 or more. In formula (1), R1 is a hydrogen atom or an alkyl group of 1 to 10 carbons, and R2 is an alkylene group of 1 to 10 carbons.
机译:根据本发明的一个方面的改性聚苯醚具有在25℃的二氯甲烷中测量的特性粘度为0.03至0.12dL / g,在其分子末端具有平均1.5至3个由式表示的基团。 (1)每分子以下,且包含不超过5质量%的分子量为13,000以上的高分子量组分。式(1)中,R 1为氢原子或碳数为1至10的烷基,R 2为碳数为1至10的亚烷基。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号