High viscosity, functionalized metallocene polyalphaolefin base stocks and processes for preparing same
High viscosity, functionalized metallocene polyalphaolefin base stocks and processes for preparing same
展开▼
机译:高粘度,官能化的茂金属聚α-烯烃基础油及其制备方法
展开▼
页面导航
摘要
著录项
相似文献
摘要
A process for producing a high viscosity functionalized metallocene polyalphaolefin (mPAO) fluid. The process includes providing a mPAO having a terminal double bond, said mPAO produced by the metallocene-catalyzed oligomerization or polymerization of an alpha-olefin feed; providing at least one of a substituted or unsubstituted alkyl thiol, aryl thiol, diphenylamine or naphthalene; and reacting, optionally in the presence of a catalyst or initiator, the mPAO having a terminal double bond with at least one of the substituted or unsubstituted alkyl thiol, aryl thiol, diphenylamine or naphthalene, under reaction conditions sufficient to produce the functionalized high viscosity mPAO fluid. The functionalized mPAO fluid has, as synthesized, a viscosity (Kv100) from 135 to 900 cSt at 100° C.; a viscosity index (VI) greater than 150; a pour point (PP) less than −25° C.; a molecular weight distribution (Mw/Mn) less than 2.0; a residual unsaturation (Bromine Number) less than 2.0; and a glass transition temperature Tg less than −30° C.
展开▼
机译:一种生产高粘度官能化的茂金属聚α烯烃(mPAO)流体的方法。该方法包括提供具有末端双键的mPAO,所述的mPAO是通过茂金属催化的α-烯烃进料的低聚或聚合反应制得的。提供取代或未取代的烷基硫醇,芳基硫醇,二苯胺或萘中的至少一种;在足以产生官能化高粘度mPAO的反应条件下,任选地在催化剂或引发剂的存在下,使具有末端双键的mPAO与取代或未取代的烷基硫醇,芳基硫醇,二苯胺或萘中的至少一种反应。体液。经合成,官能化的mPAO流体在100℃下的粘度(Kv 100 Sub>)为135至900cSt。粘度指数(VI)大于150;倾点(PP)小于-25℃;分子量分布(Mw / Mn)小于2.0;残余不饱和度(溴数)小于2.0;玻璃化温度T g Sub>小于-30℃。
展开▼