It provides a coal briquettes and a method of manufacturing the same by increasing the soft melt temperature range to improve the hot strength. The coal briquettes are charged into a molten gasifier in a molten iron manufacturing apparatus including i) a molten gasification furnace into which reduced iron is charged, and ii) a reducing gas providing the reducing iron to a molten gasifier and receiving a reducing gas from the molten gasifier. The method for producing coal briquettes includes i) mixing three or more types of coals, ii) providing a mixture of coal mixed with a binder, and iii) molding the mixture to produce coal briquettes. In the coal mixing step, the overlapping temperature range of the softening melting temperature range of the first coal and the softening melting temperature range of the second coal among the three or more types of coals may be 0 to 10 ° C.
机译:通过增加软熔温度范围以提高热强度,提供了一种煤饼及其制造方法。将煤团块装入铁水制造设备中的熔融气化炉中,该设备包括:i)向其中装入还原铁的熔融气化炉,和ii)将还原铁提供给熔融气化炉并从还原气中接收还原气体的还原气体。熔融气化炉。用于生产煤饼的方法包括:i)混合三种或更多种类型的煤,ii)提供与粘结剂混合的煤的混合物,以及iii)将混合物成型以生产煤饼。在煤混合步骤中,三种或更多种煤中的第一煤的软化熔融温度范围和第二煤的软化熔融温度范围的重叠温度范围可以为0至10℃。

著录项

  • 公开/公告号KR102023065B1

    专利类型

  • 公开/公告日2019-09-19

    原文格式PDF

  • 申请/专利权人 주식회사 포스코;

    申请/专利号KR1020170175460

  • 发明设计人 김재동;류진호;박석인;

    申请日2017-12-19

  • 分类号C10L5/14;C10L5/28;C10L5/34;

  • 国家 KR

  • 入库时间 2022-08-21 11:47:46

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号