The present invention is a boroaluminosilicate mineral material, a low-temperature co-fired ceramic composite material based on the material, a low-temperature co-fired ceramic, a composite substrate, and a method for producing the same. The boroaluminosilicate mineral material is a boroaluminosilicate mineral material for low temperature co-fired ceramics, and contains the following composition components in the following oxide-based mass percentage content indication. 0.41% to 1.15% Na 2 O, 14.15% to 23.67% K 2 O, 1.17% to 4.10% Ca O, 0 to 2.56% Al 2 O 3 , 13.19% to 20.00% B 2 O 3 , and 53.47% to 67.17% SiO 2 . Boroaluminosilicate mineral materials have stable chemical properties. The co-fired ceramics produced thereby not only have excellent dielectric properties, but also have low sintering temperature, low coefficient of thermal expansion, excellent mechanical properties and good LTCC process suitability, which makes them suitable for LTCC package substrates. Used in the field. Original text provided. [Selection diagram] Fig. 1
机译:本发明是硼铝硅酸盐矿物材料,基于该材料的低温共烧陶瓷复合材料,低温共烧陶瓷,​​复合基板及其制造方法。硼铝硅酸盐矿物材料是用于低温共烧陶瓷的硼铝硅酸盐矿物材料,并且在以下基于氧化物的质量百分比含量指示中包含以下组成成分。 Na 2 O为0.41%至1.15%,K 2 O为14.15%至23.67%,Ca O为1.17%至4.10%,Al 2为0至2.56% / Sub> O 3 ,13.19%至20.00%B 2 O 3 和53.47%至67.17%SiO 2 。硼铝硅酸盐矿物材料具有稳定的化学性质。由此制得的共烧陶瓷不仅具有优异的介电性能,而且具有低的烧结温度,低的热膨胀系数,优异的机械性能和良好的LTCC工艺适应性,这使其适合于LTCC封装基板。在现场使用。提供原始文本。 [选择图]图1

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号