The present invention relates to a method for producing an object in an additive manufacturing process from a precursor and comprises the following steps: I) depositing a layer of a radically cross-linkable construction material, which corresponds to a first selected cross-section of the precursor, on a carrier; II) depositing a layer of a radically cross-linkable construction material, which corresponds to a further selected cross-section of the precursor, on a previously applied layer of the radically cross-linked construction material; III) repeating step II) until the precursor is formed. The radically cross-linkable construction material comprises a thermoplastic radically cross-linkable polyurethane with a urethane group content of ≥5% by weight and a photoinitiator. The radically cross-linkable construction material is also heated to a processing temperature that is greater than the melting point of the radically cross-linkable polyurethane. After step III) the precursor having a temperature of 20° C. is defined as the object, or step IV) is performed: IV) performing a chemical reaction in the precursor obtained after step III) so that the object is obtained.
机译:本发明涉及一种在增材制造过程中由前体制造物体的方法,该方法包括以下步骤:I)沉积一层可自由基交联的建筑材料,该材料对应于该材料的第一选定横截面。前体,在载体上; II)在先前施加的自由基交联的建筑材料层上沉积一层自由基可交联的建筑材料,其对应于前体的进一步选择的横截面; III)重复步骤II),直到形成前体。自由基可交联的建筑材料包括具有≥5重量%的氨基甲酸酯基含量的热塑性自由基可交联的聚氨酯和光引发剂。所述可自由基交联的建筑材料也被加热至高于所述可自由基交联的聚氨酯的熔点的加工温度。在步骤III)之后,将温度为20℃的前体定义为目标,或者进行步骤IV):IV)对在步骤III)之后获得的前体进行化学反应,从而获得目标。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号