Sintering experiments on boron carbide (B4C) are performed by hot pressing (HP) and spark plasma sintering (SPS). Results show that the maximum densification rate of SPS occurs at approximately 1850 degrees C, which is earlier than that of HP. The microstructure of samples sintered by HP is very homogeneous and has a relative density of about 91%. In SPS, a high relative density of 94% can be realised, but the microstructure of the samples presents two obviously different regions. The microstructure of region I is very similar to those of samples sintered by HP. However, region II, which has a non-uniform grain size distribution, shows considerably higher relative density than region I. The mechanical properties of the samples sintered by SPS are superior to those of the samples sintered by HP because of the formation of region II.
机译:通过热压(HP)和火花等离子体烧结(SPS)进行碳化硼(B4C)的烧结实验。 结果表明,SPS的最大致密化率在大约1850摄氏度上发生,该率比HP更早。 由HP烧结的样品的微观结构非常均匀,相对密度为约91%。 在SPS,相对密度的高密度; 可以实现94%,但样品的微观结构具有两个明显不同的区域。 区域I的微观结构与由HP烧结的样品非常相似。 然而,具有非均匀晶粒尺寸分布的区域II具有比区域I相当高的相对密度。由于区域II的形成,SPS烧结的样品的机械性能优于由HP烧结的样品 。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号