Objective This study aimed to compare dentin bond durability under different degradation conditions between two etch-and-rinse (ER) systems and a universal adhesive in ER mode. Method This study used a universal adhesive [Scotchbond Universal (SU)], a three-step ER adhesive [Scotchbond Multi-Purpose Plus (SM)], and a two-step ER adhesive [Single Bond Plus (SB)]. A phosphoric acid-etching agent was applied to bovine dentin prior to the application of either a primer or the adhesive. After acid etching, bonding procedures were conducted. The specimens were divided into three group classes: (1) subjected to 10,000, 30,000, or 50,000 thermal cycles (TC); (2) stored in distilled water at 37 degrees C for 6 months or 1 year (WS); and (3) stored in distilled water for 24 h (baseline). Shear bond strength (SBS) tests were conducted. Results SB showed a higher baseline SBS than the other adhesives. Defining the baseline SBS value for each adhesive system as 100%, TC groups ranged from 56.1 to 70.3% for SM, from 98.4 to 103.7% for SB, and from 120.3 to 126.7% for SU. WS groups ranged from 66.2 to 71.4% for SM, from 98.1 to 103.3% for SB, and from 102.5 to 118.1% for SU. Conclusions Although SB showed relatively stable dentin bond performance under all degradation conditions, SM showed decreased dentin SBS with prolonged degradation. SU did not show any significant decrease in SBS from the baseline under any degradation condition.
机译:目的本研究旨在将牙本质键在两个蚀刻和冲洗(ER)系统之间的不同降解条件下的牙蛋白粘合耐久性与ER模式的通用粘合剂进行比较。该研究采用通用粘合剂[Scotchbond Universal(Su)],三步ER粘合剂[Scotchbond多功能加(SM)],以及两步ER粘合剂[单键加(SB)]。在施用底漆或粘合剂之前将磷酸蚀刻剂施加到牛牙本质中。在酸蚀刻后,进行粘合剂。将试样分为三个组类:(1)经受10,000,30,000或50,000个热循环(Tc); (2)在37摄氏度储存在蒸馏水6个月或1年(WS); (3)储存在蒸馏水24小时(基线)。进行剪切粘合强度(SBS)测试。结果SB显示比其他粘合剂更高的基线SBS。将每个粘合剂系统的基线SBS值定义为100%,TC组的SM为56.1至70.3%,SB的98.4至103.7%,苏为40.3%至126.7%。 SM的36.2%至71.4%的范围从98.1至103.3%的SB,苏的102.5%至118.1%。结论虽然Sb在所有降解条件下表现出相对稳定的牙本质键性能,但SM显示牙本质SBS降低,延长了降解。在任何降解条件下,苏未显示出从基线的SBS中的任何显着降低。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号