Bleaching Kinetic and Mechanism Study of Congo Red Catalyzed by ZrO2 Nanoparticles Prepared by Using a Simple Precipitation Method

机译:简单沉淀法制备的ZrO2纳米粒子催化刚果红的漂白动力学及机理研究

获取原文
获取原文并翻译 | 示例
           

摘要

Bleaching of Congo red catalyzed by ZrO2 nanoparticles was study under UV and sunlight irradiations. The nanoparticles of ZrO2 have been synthesized by controlled precipitation method. The concentration of ZrOCl2 and ammonia reac-tants and the calcinations temperature of ZrO2 were optimized for the control of nanoparticles size. Characterization of the prepared nanoparticles was studied by using XRD patterns, TEM images and FT-IR spectra. The tetragonal phase of zirconium oxide was obtained at 550 °C and show the most catalytic effect in dye degradation. The various parameters such as the irradiation time, amount of nanophotocatalyst, pH of samples, and initial concentration of Congo red were studied to find desired conditions of photodegradation process. The degradation 98% was achieved at pH 7 catalyzed by 0.7 g/L if ZrO2 nanoparticles in duration time of 125 min. The effect of iso-PrOH, hydrogen peroxide and inorganic anions was studied on the degradation efficiency of dye. The degradation 98% was obtained in the presence of prepared nanosized zirconia in comparison with degradation 65% catalyzed by commercially zirconia.
机译:在紫外线和阳光照射下,研究了ZrO2纳米粒子催化的刚果红漂白。 ZrO2纳米粒子已通过控制沉淀法合成。优化了ZrOCl2和氨反应物的浓度以及ZrO2的煅烧温度,以控制纳米粒子的大小。使用XRD图谱,TEM图像和FT-IR光谱研究了制备的纳米颗粒的表征。氧化锆的四方相是在550°C下获得的,在染料降解中表现出最大的催化作用。研究了各种参数,例如辐照时间,纳米光催化剂的量,样品的pH值和刚果红的初始浓度,以找到所需的光降解过程条件。如果ZrO2纳米粒子在125分钟的持续时间内,在0.7 g / L的pH 7催化下,降解率达到98%。研究了异PrOH,过氧化氢和无机阴离子对染料降解效率的影响。在制备的纳米级氧化锆的存在下,相比于商业氧化锆催化的65%的降解,获得98%的降解。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号