首页> 外文期刊>Journal of the European Ceramic Society >Oxidation behaviour of SiC/SiC ceramic matrix composites in air
【24h】

Oxidation behaviour of SiC/SiC ceramic matrix composites in air

机译:SiC / SiC陶瓷基复合材料在空气中的氧化行为

获取原文
获取原文并翻译 | 示例

摘要

Oxidation of silicon melt infiltrated SiC/SiC ceramic matrix composites (CMC) was studied in air at 1200-1400 degrees C for 1, 5, 24 and 48 h. Weight gain and oxide layer thickness measurements revealed the oxidation follows parabolic reaction kinetics with increase in temperature and time. XRD showed the extent of oxide layer (SiO2) formation was greatest after 4811 at 1400 degrees C: an observation confirmed by X-ray photoelectron spectroscopy (XPS), energy dispersive spectroscopy (EDS) and transmission electron microscopy (TEM) analyses. Oxide layer thickness varied from 1 mu m after 48 hat 1200 degrees C to 8 mu m after 48 h at 1400 degrees C. Oxidation of SiC/SiC composites is both temperature and time dependent with an activation energy of 619 kJ mol(-1). BN coatings around SiC fibres showed good resistance to oxidation even after 48 hat 1400 degrees C. (C) 2016 Elsevier Ltd. All rights reserved.
机译:研究了硅熔体渗入的SiC / SiC陶瓷基复合材料(CMC)在1200-1400摄氏度的空气中氧化1、5、24和48 h的过程。重量增加和氧化物层厚度测量表明,氧化遵循抛物线反应动力学,随温度和时间的增加而增加。 XRD显示,在1400℃下4811之后,氧化层(SiO2)的形成程度最大:通过X射线光电子能谱(XPS),能量色散能谱(EDS)和透射电子显微镜(TEM)分析证实了这一观察结果。氧化层厚度从1200摄氏度的48帽后的1微米变化到1400摄氏度的48小时后的8微米。SiC / SiC复合材料的氧化过程受温度和时间的影响,活化能为619 kJ mol(-1)。 。 SiC纤维周围的BN涂层即使在48帽1400摄氏度后仍显示出良好的抗氧化性。(C)2016 Elsevier Ltd.保留所有权利。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号