The aim of this study was to investigate the effect of adding powdered dentin to primer or adhesive in a self-etch system on the shear bond strength of three resin-based sealers. Seventy-two premolars were sectioned buccolingually, and 144 root halves were divided into three groups according to the sealer used: epoxy resin-based sealer (AH Plus), methacrylate resin-based (RealSeal, Hybrid Root SEAL) n=48. The surfaces were irrigated with 5% NaOCl, 17% EDTA, distilled water for 5min. Four subgroups were created (n=12): control group; Clearfil Liner Bond 2V treated group; powdered dentin added to the primer of Clearfil Liner Bond 2V (40 wt.%); and powdered dentin added to the adhesive of Clearfil Liner Bond 2V (20 wt.%). Dentin powder was prepared. Three mm high buildups with a constant surface area of 3.45mm(2) were created using the sealers and allowed to set (37oC, 100% humid, 72h). The samples were tested to failure for shear bond strength (1mm/min). The data were calculated (MPa) and analyzed using two-way ANOVA, one-way ANOVA, and Tukey HSD tests. Adhesive use decreased the bonding performance of AH Plus (p=0.00). Mean bond strength of the other sealers was found similar to control. Primer or adhesive resin with powdered dentin did not increase the adhesive performance of the self-etch system used. The shear bond strength of RealSeal was significantly increased when powdered dentin was added to primer or adhesive (p=0.00). The effect of adding powdered-dentine to primer or adhesive in a self-etch system on the shear bond strength was sealer-dependent .
机译:这项研究的目的是研究在自蚀刻系统中将粉状牙本质添加到底漆或粘合剂中对三种树脂基密封剂的剪切粘合强度的影响。根据口头切开术将72颗前磨牙切开,将144个根半部分分为三组:基于环氧树脂的密封剂(AH Plus),基于甲基丙烯酸酯的密封剂(RealSeal,Hybrid Root SEAL)n = 48。用5%NaOCl,17%EDTA,蒸馏水冲洗表面5分钟。创建了四个亚组(n = 12):对照组; Clearfil Liner Bond 2V治疗组;将粉状牙本质添加到Clearfil Liner Bond 2V的底漆中(40 wt。%);然后将粉状的牙本质添加到Clearfil Liner Bond 2V(20 wt。%)的粘合剂中。制备牙本质粉。使用密封剂创建了3毫米高的堆积物,其恒定表面积为3.45毫米(2),并被设定为(37oC,100%湿度,72h)。测试样品的剪切粘合强度(1mm / min)失败。计算数据(MPa),并使用双向ANOVA,单向ANOVA和Tukey HSD测试进行分析。粘合剂的使用会降低AH Plus的粘合性能(p = 0.00)。发现其他密封剂的平均粘合强度与对照相似。带有粉状牙本质的底漆或粘合树脂不会提高所用自蚀刻系统的粘合性能。当将粉状牙本质添加到底漆或粘合剂中时,RealSeal的剪切粘合强度显着提高(p = 0.00)。在自蚀刻系统中向底漆或粘合剂中添加牙粉粉对剪切粘结强度的影响取决于密封剂。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号