Effect of dentine smear layer on the performance of self-etching adhesive systems: A micro-tensile bond strength study

机译:牙本质涂抹层对自蚀刻胶粘剂系统性能的影响:微拉伸粘合强度研究

获取原文
获取原文并翻译 | 示例
           

摘要

This study aimed to evaluate the effect of the smear layer on the micro-tensile bond strength when two self-etching adhesives were used with different techniques. Flat dentine surfaces were prepared using either medium grit diamond burs or tungsten carbide burs. Ten specimens from each prepared surfaces were subjected for smear layer evaluation under SEM. Forty specimens from each of the prepared surfaces were further divided into two groups, bonded with either Clearfil SE Bond (SE) or Clearfil S3 Bond (S3) using one of four applications (as manufacturer's instructions, agitation, reapplication, and increased application time), restored with composites and subjected to a micro-tensile bond strength test. Smear layers created with diamond burs were thicker than those created with tungsten carbide burs. Surfaces prepared with tungsten carbide burs produced a higher bond strength than those prepared with diamond burs and the same type of adhesive resin. SE demonstrated a higher bond strength than S3 for all surfaces. S3 applied with the agitation technique demonstrated a higher bond strength to dentine prepared with tungsten carbide and diamond burs than that applied with other techniques. SE applied with increased time on dentine treated with carbide burs produced the highest bond strength. In conclusion, a thick smear layer decreased bond strength to dentine, and this might be improved by modification of application technique.
机译:这项研究旨在评估在两种自蚀刻粘合剂以不同技术使用时涂片层对微拉伸粘合强度的影响。使用中等粒度的金刚石车针或碳化钨车针制备平坦的牙本质表面。来自每个准备好的表面的十个样品在SEM下进行涂片层评估。将来自每个准备好的表面的40个样品进一步分为两组,使用四个应用程序之一(按照制造商的说明,搅拌,重新应用程序和增加的应用程序时间),用Clearfil SE Bond(SE)或Clearfil S3 Bond(S3)进行粘合。 ,用复合材料修复,并进行了微拉伸粘合强度测试。用金刚石钻头形成的涂片层比用碳化钨钻头形成的涂片层厚。用碳化钨钻头制备的表面比使用金刚石钻头和相同类型的粘合树脂制备的表面具有更高的结合强度。 SE在所有表面上均表现出比S3更高的结合强度。搅拌技术应用的S3与使用碳化钨和金刚石钻头制备的牙本质相比,其结合强度更高。 SE随碳化物磨头处理的牙本质的添加时间增加而产生最高的结合强度。总之,较厚的涂片层会降低与牙本质的粘合强度,可以通过修改涂布技术来改善。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号