Recently, material of Inconel 690TT (thermal treatment) for the steam generator tubes in a nuclear power plant was substituted for the existing material of Inconel 600HTMA (high temperature mill-annealing). Inconel 690TT has more chromium than Inconel 600HTMA in order to improve the corrosion resistance. In this study, to evaluate the friction and wear characteristics of Inconel 690TT under fretting condition, the fretting tests as well as sliding tests were carried out in air and in elevated temperature water environment, respectively. Fretting tests of the cross-cylinder type were done under various applied normal loads, and sliding tests of pin-on-disk type were also carried out to compare with the results of the fretting test. In summary, the results of the fretting tests correlated with the results of the sliding tests. The wear mechanism of Inconel 690TT in air was delamination wear and the mechanism in water was affected by micro-pitting. Also, it was found that the fretting wear coefficients in water were increased with increase in the temperature of water.
机译:最近,用于核电站蒸汽发生器管的Inconel 690TT(热处理)材料替代了Inconel 600HTMA(高温轧机退火)的现有材料。为了提高耐腐蚀性,Inconel 690TT比Inconel 600HTMA具有更多的铬。在这项研究中,为了评估Inconel 690TT在微动条件下的摩擦和磨损特性,分别在空气和高温水环境中进行了微动试验和滑动试验。在各种施加的正常载荷下进行了跨圆柱型的微动试验,还进行了销盘式的滑动试验,以与微动试验的结果进行比较。总之,微动试验的结果与滑动试验的结果相关。 Inconel 690TT在空气中的磨损机理为分层磨损,而在水中的磨损机理则受到微点蚀的影响。另外,还发现随着水温的升高,水中的微动磨损系数增加。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号