In order to recover chromium from vanadium slag, the leaching behaviour of chromium during vanadium extraction was studied. The effects of the several parameters that included roasting temperature, roasting time, types of additives as well as addition mass of additives were investigated. The results indicated that chromium can be leached at the same time during vanadium leaching from vanadium slag. In comparison, under the same conditions, the leaching of vanadium is easier than that of chromium. The leaching rate of vanadium and chromium can be beyond 96 and 91%, respectively, under the experimental condition of roasting temperature of 700°C, roasting time of 2 h, 30% (mass fraction) sodium chloride and 20% (mass fraction) sodium carbonate addition to the vanadium slag, leaching temperature of 95°C, and leaching time of 3 h.
机译:为了从钒渣中回收铬,研究了钒萃取过程中铬的浸出行为。研究了焙烧温度,焙烧时间,添加剂种类以及添加剂添加量等几个参数的影响。结果表明,从钒渣中浸出钒的过程中铬可以同时浸出。相比之下,在相同条件下,钒的浸出比铬的浸出更容易。在焙烧温度700℃,焙烧时间2 h,氯化钠(质量分数)30%和氯化钠(质量分数)20%的实验条件下,钒和铬的浸出率分别可以超过96%和91%。向钒渣中添加碳酸钠,浸出温度为95°C,浸出时间为3 h。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号