摘要

Gravimetry experiments in a well-controlled environment have been performed to investigate aging for a glassy PMMA/toluene film. The temperature is constant and the control parameter is the solvent vapor pressure above the film (i.e. the activity). Several experimental protocols have been used, starting from a high activity where the film is swollen and rubbery and then aging the film at different activities below the glass transition. Desorption and resorption curves have been compared for the different protocols, in particular in terms of the softening time, i.e. the time needed by the sample to recover an equilibrium state at high activity. Non-trivial behaviors have been observed, especially at small activities (deep quench). A model is proposed, extending the Leibler-Sekimoto approach to take into account the structural relaxation in the glassy state, using the Tool formalism. This model well captures some of the observed phenomena, but fails in describing the specific kinetics observed when aging is followed by a short but deep quench.
机译:已经在良好控制的环境中进行了重量分析实验,以研究玻璃状PMMA /甲苯膜的老化。温度是恒定的,控制参数是膜上方的溶剂蒸气压(即活性)。已经使用了几种实验方案,从高活性开始,在该高活性下,膜溶胀且具有橡胶性,然后在玻璃化转变温度以下以不同的活性使膜老化。已经针对不同方案比较了解吸和再吸收曲线,特别是在软化时间方面,即在高活性下样品恢复平衡状态所需的时间。已经观察到非平凡的行为,尤其是在小活动(深度淬火)下。提出了一个模型,使用工具形式主义扩展了Leibler-Sekimoto方法,以考虑玻璃态的结构松弛。该模型很好地捕捉了一些观察到的现象,但是未能描述在老化之后进行短暂但深度的淬火后观察到的特定动力学。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号