Tooth Enamel Evaluation After Tooth Bleaching With Hydrogen Peroxide Assisted by a DC Nonthermal Atmospheric-Pressure Plasma Jet

机译:直流非热常压等离子体射流辅助过氧化氢漂白后的牙釉质评估

获取原文
获取原文并翻译 | 示例

摘要

The purpose of this study is to evaluate the changes in dental enamel (morphology, elemental composition, microhardness, and roughness) after applying hydrogen peroxide in conjunction with a nonthermal plasma to bleach the teeth. Extracted human teeth were randomly placed in six groups. Two control groups (one group with no bleaching agent and no plasma treatment of the teeth and another one with only hydrogen peroxide as the bleaching agent) and four plasma groups (receiving hydrogen peroxide of varying concentrations 6$%$ , 15$%$, 25$ %$, and 35$%$, in conjunction with a plasma treatment) were prepared. The surface morphology before and after treatment was assessed using a scanning electron microscope (SEM), and the change in the elemental composition was analyzed by an energy-dispersive X-ray spectroscopy system. A total of 36 extracted teeth were used to evaluate the change in enamel microhardness and surface roughness. The use of hydrogen peroxide as a bleaching agent, even in the absence of plasma exposure, causes various etching patterns that are attributable to demineralization during the treatment process. These patterns are more pronounced as the hydrogen peroxide concentration increases. The surface roughness tests confirmed the findings from the SEM analysis. We only found minor essentially insignificant changes in the elemental composition of the enamel and in the surface microhardness as a result of the treatment using hydrogen peroxide and a cold plasma. The use of a cold plasma in conjunction with hydrogen peroxide of varying concentrations in tooth bleaching causes minor changes in the tooth enamel changes that are comparable to those resulting from the standard treatment using 35 $%$ hydrogen peroxide gel without a plasma.
机译:这项研究的目的是评估在与非热等离子体结合使用过氧化氢漂白牙齿后,牙釉质的变化(形态,元素组成,显微硬度和粗糙度)。将拔出的人类牙齿随机分为六组。两个对照组(一组不使用漂白剂,不对牙齿进行等离子体处理,另一组仅使用过氧化氢作为漂白剂)和四个血浆组(接收不同浓度的过氧化氢6%,15%,制备25%和35%,结合等离子体处理。使用扫描电子显微镜(SEM)评估处理前后的表面形态,并通过能量色散X射线光谱系统分析元素组成的变化。总共使用了36个拔出的牙齿来评估牙釉质显微硬度和表面粗糙度的变化。即使在没有等离子体暴露的情况下,使用过氧化氢作为漂白剂也会导致各种蚀刻图案,这些图案可归因于处理过程中的脱矿质。随着过氧化氢浓度的增加,这些模式更加明显。表面粗糙度测试证实了SEM分析的发现。由于使用过氧化氢和冷等离子体的处理,我们仅发现搪瓷的元素组成和表面显微硬度有微小的本质上微不足道的变化。冷等离子体与漂白剂中浓度不同的过氧化氢一起使用会导致牙齿珐琅质的细微变化,这与使用35 %%的无血浆过氧化氢凝胶进行标准处理所产生的变化相当。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号