Cement industry is seeking alternative raw material and process to reduce the energy consumption and environmental impacts from conventional cement manufacture. This paper describes process of belite cements synthesis. Geothermal sludges, an undesired waste from Dieng Geothermal Power Plant as amorphous silica source and calcium hydroxide were used to form belite cement at elevated temperatures. Experimental results showed that principal phase of belite cement (larnite or β-Ca_(2)SiO_(4)) was formed at temperature as low as 800 °C. Thus, the geothermal silica is shown to be very promising starting material for the low-temperature production of belite cement.
机译:水泥行业正在寻求替代性原材料和工艺,以减少常规水泥生产中的能源消耗和环境影响。本文介绍了贝利特水泥的合成过程。地热污泥,来自Dieng地热发电厂的不希望有的废物(作为无定形二氧化硅源)和氢氧化钙被用于在高温下形成贝利特水泥。实验结果表明,在低至800°C的温度下形成了贝利特水泥的主相(拉尼石或β-Ca_(2)SiO_(4))。因此,地热二氧化硅被证明是用于贝利特水泥的低温生产的非常有希望的起始材料。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号