In this study, spray-coating has been opted to prepare patterned Poly(3,4-ethylenedioxythiophene) (PEDOT) electrodes for an organic thin film transistor (OTFT). The conducting polymer was grown via the vapor phase polymerization (VPP) method. The film quality of VPP-PEDOT critically relies on the uniformity of oxidant film selectively patterned on a thermally oxidized Si-wafer surface prior to the polymerization. Therefore, to improve the uniformity of the oxidant film, this study tried to discover best conditions of spray-coating. Several different temperatures of Si-wafer substrate, distances from nozzle to wafer, and spray times were tested during the spray coating process. Then, sprayed oxidant films and vapor phase-polymerized PEDOT patterns were characterized by several thin film analyzing tools such as FE-SEM and optical microscope. The characterization found that the best conditions of spray coating are room temperature, 18 cm, and 50 s of substrate temperature, spray distance, and time, respectively.
机译:在这项研究中,已选择喷涂以制备用于有机薄膜晶体管(OTFT)的图案化聚(3,4-乙撑二氧噻吩)(PEDOT)电极。导电聚合物通过气相聚合(VPP)方法生长。 VPP-PEDOT的膜质量关键取决于聚合之前在热氧化的硅晶圆表面选择性地构图的氧化剂膜的均匀性。因此,为了提高氧化膜的均匀性,本研究试图发现喷涂的最佳条件。在喷涂过程中测试了几种不同温度的硅晶圆基板,喷嘴到晶圆的距离以及喷涂时间。然后,通过FE-SEM和光学显微镜等几种薄膜分析工具对喷涂的氧化膜和气相聚合的PEDOT图案进行了表征。该特性发现,喷涂的最佳条件分别是室温,18 cm和50 s的基材温度,喷涂距离和时间。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号