The behaviour of long tension reinforcement laps

机译:长张力增强圈的行为

获取原文
获取原文并翻译 | 示例
       

摘要

Over time, the length of reinforcement laps required by design standards has increased significantly. By way of illustration, fib Model Code 2010 can require over twice the lap length required by the superseded UK code BS 8110-1:1997. The need for this increase is debatable since, outside the laboratory, there is no evidence that laps designed to BS 8110-1: 1997 are unsafe. This paper describes an experimental programme undertaken to compare the failure modes of beams with laps of varying length loaded in four-point bending. The tested laps were classified as 'short', 'long' or 'very long', with long laps just sufficient to develop reinforcement yield. The very long laps were between 1.5 and 2.0 times the length of the long laps. The tested laps were between bars of equal as well as mixed diameter, with diameters in the range 16-25 mm. Instrumentation included strain gauges and digital image correlation, which was used to record crack development. Bond failure was very sudden and brittle in the short laps. The failure modes of both long and very long laps were ductile due to flexural reinforcement yield. However, bond failure occurred subsequent to yield in long laps including at least one 25 mm diameter bar.
机译:随着时间的流逝,设计标准要求的加固圈长度已大大增加。作为说明,fib型号代码2010可能需要超过被取代的英国代码BS 8110-1:1997所要求的圈长的两倍以上。对于这种增加的需求是有争议的,因为在实验室外,没有证据表明按照BS 8110-1:1997设计的护圈是不安全的。本文介绍了一个实验程序,该程序用于比较四点弯曲荷载下长度不同的搭接梁的破坏模式。测试的圈数分为“短”,“长”或“很长”,长圈刚好足以增强补强。很长的圈数是长圈长度的1.5到2.0倍。测试的棉卷在等直径和混合直径的棒之间,直径范围为16-25毫米。仪器包括应变仪和数字图像相关性,用于记录裂纹的发展。粘结失效非常突然,并且在短时间内变脆。由于弯曲钢筋屈服,长和长圈的失效模式都是延性的。但是,粘结失败发生在长屈服之后,包括至少一根直径为25 mm的钢筋。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号