Effects of Moist Aggregates on the Performance of Warm Mix Asphalt Mixtures Containing Non-Foaming Additives

机译:湿骨料对含非发泡添加剂的热拌沥青混合料性能的影响

获取原文
获取原文并翻译 | 示例

摘要

The objective was to conduct a laboratory investigation of moisture susceptibility and rutting resistance of non-foaming warm mix asphalt (WMA) mixtures containing moist aggregates. Gyration number and weight loss of various samples, indirect tensile strength (ITS), tensile strength ratio (TSR), rut depths of dry and moisture conditioned specimens, as well as failed temperatures and rutting factors of recovered binders were measured for all mixtures. The experimental design included two aggregate moisture contents (0 and ~0.5 % by weight of the dry mass of the aggregate), two lime contents (1 and 2 % lime by weight of dry aggregate) and one liquid anti-stripping agent (ASA), three non-foaming WMA additives (Cecabase?, Evotherm , and Rediset?) with control, and two aggregate sources. A total of 34 mixtures were designed and a total of 340 specimens were tested in this study. The test results indicated that the aggregate source significantly affects the ITS and rutting resistance regardless of the WMA additive, ASA, and moisture content. In addition, the ITS and rut depth of the non-foaming WMA mixtures containing moist aggregates generally satisfied the demand of pavement without additional treatment. The mixtures with three WMA additives exhibited similar rutting resistance under dry and wet conditions. The liquid ASA, used in this study, for moisture resistance is not recommended to use in WMA mixtures containing moist aggregates as the aggregate is sensitive to moisture.
机译:目的是对含有湿集料的非发泡温拌沥青混合料(WMA)的湿气敏感性和耐车辙性进行实验室研究。测量了所有混合物的各种样品的回转数和重量损失,间接拉伸强度(ITS),拉伸强度比(TSR),干燥和湿润条件的样品的车辙深度以及失效的温度和回收粘合剂的车辙因子。实验设计包括两种集料水分含量(分别为集料干重的0%和〜0.5%),两种石灰含量(干集料重量为1%和2%石灰)和一种液体防剥离剂(ASA) ,三种非发泡WMA添加剂(Cecabase?,Evotherm和Rediset?)和对照,以及两种聚合来源。本研究共设计了34种混合物,并测试了340个样品。测试结果表明,无论WMA添加剂,ASA和水分含量如何,骨料来源都会显着影响ITS和耐车辙性。另外,含有湿性骨料的非发泡WMA混合物的ITS和车辙深度通常无需进一步处理即可满足路面需求。具有三种WMA添加剂的混合物在干燥和潮湿条件下均表现出相似的耐车辙性。不建议将本研究中用于防潮的液体ASA用于含有潮湿聚集体的WMA混合物中,因为聚集体对水分敏感。

著录项

  • 来源
    《Journal of testing and evaluation》 |2011年第5期|p.847|共1页
  • 作者单位

    Ph.D., Post-Doctoral Research Fellow, Department of Civil Engineering,Clemson University, Clemson, SC 29634-0911.;

    Ph.D., P.E., Research Assistant Professor, Asphalt Rubber Technology Service (ARTS), Department of Civil Engineering, Clemson University, Clemson,SC 29634-0911 (Corresponding author);

    Ph.D., Consultant, Guest Professor, Key Laboratory of Silicate Materials Science and Engineering of Ministry of Education, Wuhan Univ. of Technology,Wuhan 430070, China;

  • 收录信息 美国《科学引文索引》(SCI);美国《工程索引》(EI);
  • 原文格式 PDF
  • 正文语种 eng
  • 中图分类
  • 关键词

    warm mix asphalt; tensile strength ratio; moisture susceptibility; rutting resistance;