Repair of rabbit femoral condyle bone defects with injectable nanohydroxyapatite/chitosan composites

机译:可注射纳米羟基磷灰石/壳聚糖复合材料修复兔股骨dy骨缺损

获取原文
获取原文并翻译 | 示例
           

摘要

Repair of massive bone loss remains a challenge to the orthopaedic surgeons. Autologous and allo-genic bone grafts are choice for bone reconstructive surgery, but limited availability, risks of transmittable diseases and inconsistent clinical performances have prompted the development of tissue engineering. In the present work, the bone regeneration potential of nanohydroxyapatite/chitosan composite scaffolds were compared with pure chitosan scaffolds when implanted into seg-mental bone defects in rabbits. Critical size bone defects (6 mm diameter, 10 mm length) were created in the left femoral condyles of 43 adult New Zealand white rabbits. The femoral condyle bone defects were repaired by nanohydroxyapatite/chitosan compositions, pure chitosan or left empty separately. Defect-bridging was detected by plain radiograph and quantitative computer tomography at eight and 12 weeks after surgery. Tissue samples were collected for gross view and histological examination to determine the extent of new bone formation. Eight weeks after surgery, more irregular osteon formation was observed in the group treated with nanohydroxyapatite/chitosan composites compared with those treated with pure chitosan. 12 weeks after surgery, complete healing of the segmental bone defect was observed in the nanohydroxyapatite/chit-osan-group, while the defect was still visible in the chitosan-group, although the depth of the defect had diminished. These observations suggest that the injectable nanohydroxyapatite/chitosan scaffolds are potential candidate materials for regeneration of bone loss.
机译:修复大量骨丢失仍然是整形外科医生的挑战。自体和同种异体骨移植物是进行骨重建手术的选择,但是可用性有限,可传播疾病的风险以及临床表现的不一致促使组织工程学的发展。在目前的工作中,当将纳米羟基磷灰石/壳聚糖复合支架植入兔的节段性骨缺损中时,将其与纯壳聚糖支架进行了骨再生。在43只成年新西兰白兔的左股骨con中产生了临界尺寸的骨缺损(直径6毫米,长度10毫米)。用纳米羟基磷灰石/壳聚糖组合物,纯壳聚糖修复股骨dy骨缺损或单独排空。术后8周和12周通过X线平片和定量计算机X线断层摄影术检测缺陷桥接。收集组织样品以进行总体观察和组织学检查,以确定新骨形成的程度。术后八周,与纯壳聚糖相比,纳米羟基磷灰石/壳聚糖复合物治疗组的骨质形成更为不规则。术后12周,在纳米羟基磷灰石/壳聚糖组中观察到节段性骨缺损的完全愈合,而在壳聚糖组中该缺损仍可见,尽管缺损的深度已减小。这些观察结果表明,可注射的纳米羟基磷灰石/壳聚糖支架是骨丢失再生的潜在候选材料。

著录项

  • 来源
    《Journal of materials science》 |2012年第8期|p.1941-1949|共9页
  • 作者单位

    Department of Orthopaedics, Zhu Jiang Hospital, Southern Medical University, No. 253, Gongye Big Road, Guangzhou 510282, China;

    Department of Orthopaedics, Zhu Jiang Hospital, Southern Medical University, No. 253, Gongye Big Road, Guangzhou 510282, China;

    Department of Orthopaedics, Zhu Jiang Hospital, Southern Medical University, No. 253, Gongye Big Road, Guangzhou 510282, China;

    Department of Orthopaedics, Zhu Jiang Hospital, Southern Medical University, No. 253, Gongye Big Road, Guangzhou 510282, China;

    Xiang Yang Central Hospital, Jingzhou Street, Xiangyang 441021, Hubei, China;

    Qinghai University Affiliated Hospital, No. 29, Tongren Road,Xining 810001, Qinghai, China;

    Department of Orthopaedics, Zhu Jiang Hospital, Southern Medical University, No. 253, Gongye Big Road, Guangzhou 510282, China;

    Department of Orthopaedics, Zhu Jiang Hospital, Southern Medical University, No. 253, Gongye Big Road, Guangzhou 510282, China;

  • 收录信息
  • 原文格式 PDF
  • 正文语种 eng
  • 中图分类
  • 关键词

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号