The adoption of warm mix asphalt (WMA) technologies is well accepted due to its promising environmental benefits, however, their long-term field performance is not well understood. This study focused on the long-term rutting resistance of WMA and their companion hot mix asphalt (HMA) based on 83 field samples collected from 28 field projects across the United States covering four climate zones, and quantified environmental impacts for various WMA technologies as compared to HMA. Field cores were evaluated by dynamic modulus, creep compliance, and Hamburg wheel-tracking device tests. Asphalt binders extracted from field cores were evaluated by continuous performance grading (PG), multiple stress creep recovery (MSCR), and monotonic shear tests. The results showed that WMA binders exhibited similar rutting resistance compared with the HMA binders after long-term field aging. Existence of polymer in the asphalt binder was displayed through the plot of non-recoverable creep compliance and percent recovery. The long-term field aged polymer modified asphalt binders for WMA and HMA were comparable. The results also showed that the CO2 reduction by using WMA ranged from 89.09% to 42.79% depending on WMA type. On average, the CO2 emission was reduced to 66.89% by using WMA technologies. Overall, environmental impact analysis and long-term field performance results validated the confident use of WMA technologies. (C) 2020 Elsevier Ltd. All rights reserved.
机译:由于其有前途的环境效益,采用温暖的混合沥青(WMA)技术得到很好地接受,但其长期现场性能并不充分了解。本研究专注于WMA及其同伴热混合沥青(HMA)的长期车辙抗性,基于来自美国的28个田间项目的83个田间样本,涵盖四个气候区域,并与各种WMA技术相比量化的环境影响到HMA。通过动态模量,蠕变顺应性和汉堡轮跟踪装置测试评估现场核心。通过连续性能分级(PG),多重应力蠕变恢复(MSCR)和单调剪切试验评估从野外核中提取的沥青粘合剂。结果表明,与长期田间老化后的HMA粘合剂相比,WMA粘合剂表现出类似的车辙抗性。通过不可恢复的蠕变顺应性的曲线显示沥青粘合剂中聚合物的存在性和百分比回收率。用于WMA和HMA的长期场老化聚合物改性沥青粘合剂是可比的。结果还表明,根据WMA型,使用WMA的CO 2减少了89.09%至42.79%。平均而言,通过使用WMA技术,CO2排放减少到66.89%。总体而言,环境影响分析和长期现场绩效结果验证了自信地使用WMA技术。 (c)2020 elestvier有限公司保留所有权利。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号