Data from the thermal depolymerization of polystyrene in a highly aromatic hydrocarbon medium (light and heavy cycle oil) have been obtained. The influences of the reaction conditions on the conversion and selectivity have been studied. The maximum yield of styrene obtained in the present work is 84.4% at a polymer conversion of 93.8% in light cycle oil under the following conditions: temperature: 500 degrees C, vapor residence time: 2.61 s, polymer concentration: 15%. The styrene yield obtained is higher than has been previously reported in the scientific literature. The high selectivity of styrene in the depolymerization reaction can be explained by the fact that under the reaction conditions studied, the formation of styrene dimers in the hydrocarbon medium is inhibited.
机译:从聚苯乙烯在高度芳族烃介质(轻和重循环油)中的热解聚获得了数据。研究了反应条件对转化率和选择性的影响。在以下条件下,在轻循环油中,聚合物转化率为93.8%,在本工作中获得的苯乙烯最大产率为84.4%:温度:500摄氏度,蒸气停留时间:2.61 s,聚合物浓度:15%。所获得的苯乙烯收率高于科学文献中先前报道的收率。可以通过以下事实来解释解聚反应中苯乙烯的高选择性:在所研究的反应条件下,可以抑制烃介质中苯乙烯二聚体的形成。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号