Objective: This clinical study was conducted in order to evaluate force decay over time of latex and non-latex orthodontic intraoral elastics. Methods: Patients (n = 15) were evaluated using latex and non-latex elastics in the periods of : 0, 1, 3, 12 and 24 hours. The rubber bands were transferred to the testing machine (EMIC DL-500 MF), and force values were recorded after stretching the elastic to a length of 25mm. Paired t test was applied and analysis of variance (ANOVA) was used to evaluate the variation of force generated. LSD (Fisher’s least significant difference) post-hoc test was thus employed. Results: As regards the initial forces (zero time), the values of force for non-latex elastic were slightly higher than for the latex elastic. In the subsequent times, the forces generated by the latex elastic showed higher values. Regarding the material degradation, at the end of 24 hours the highest percentage was observed for non-latex elastic. Conclusions: The latex elastics had a more stable behavior during the studied period, compared with non-latex.
机译:目的:进行这项临床研究以评估乳胶和非乳胶正畸口腔内弹性随时间的力衰减。方法:在15、0、1、3、12和24小时内使用乳胶和非乳胶弹性材料对患者(n = 15)进行评估。将橡皮筋转移到测试机(EMIC DL-500 MF),并在将弹性体拉伸至25mm的长度后记录力值。应用配对t检验,并使用方差分析(ANOVA)评估所产生力的变化。因此,采用了LSD(Fisher最小显着差异)事后测试。结果:关于初始力(零时间),非乳胶弹性体的力值略高于乳胶弹性体。在随后的时间里,由乳胶弹性产生的力显示出更高的值。关于材料降解,在24小时结束时观察到非乳胶弹性的百分比最高。结论:与非乳胶相比,乳胶弹性体在研究期间具有更稳定的行为。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号