This article presents results of an experimental study on the sphalerite activation with Cu(II) and Pb(II), whose main objective was to investigate the activation mechanisms and to evaluate the magnitude of the hydrophobization achieved with both chemical species. The hydrophobicity acquired by the mineral due to the interaction with the activator and collector (sodium isopropyl xanthate) is characterized making use of the contact angle technique. The results show that Cu(II) replaces the Zn of the external layers of the mineral, promoting the sulfide (S 2– ) oxidation to produce a mixture of CuS, Cu 2 S and S°, of hydrophobic nature. The subsequent interaction with xanthate increases the hydrophobicity of the mineral surface. In turn, Pb(II) activation of sphalerite is due to the formation of a PbS layer that reacts with xanthate to produce hydrophobic species (e.g., PbX 2 ). It is also observed that the hydrophobicity of sphalerite activated with Pb(II) is favored under air atmospheres, as compared to that obtained under nitrogen atmospheres. It is concluded that the hydrophobicity achieved by lead activation may be of the same order of magnitude to that deliverately induced by copper activation.
机译:本文介绍了用Cu(II)和Pb(II)活化闪锌矿的实验研究结果,其主要目的是研究活化机理并评估两种化学物质实现的疏水化程度。矿物由于与活化剂和捕收剂(异丙基黄原酸钠)的相互作用而获得的疏水性利用接触角技术进行了表征。结果表明,Cu(II)替代了矿物外层的Zn,从而促进了硫化物(S 2–)的氧化,从而生成了具有疏水性的CuS,Cu 2 S和S°的混合物。随后与黄药的相互作用增加了矿物表面的疏水性。继而,闪锌矿的Pb(II)活化是由于形成了与黄药发生反应以产生疏水性物质(例如PbX 2)的PbS层。还观察到,与在氮气氛下获得的相比,在空气气氛下被Pb(II)活化的闪锌矿的疏水性是有利的。结论是,通过铅活化获得的疏水性可以与通过铜活化传递的疏水性具有相同的数量级。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号