The experiments proved that during a thermal runaway, hydrogen is evolved from sealed nickel–cadmium batteries in amount approximately ten times less than from unsealed batteries of the samecapacity equipped with electrodes of the same type. Besides, the electrodes of the sealed nickel–cadmium batteries with a long operating life contain an amount of hydrogen 10-12 times less than thesimilar unsealed batteries.