首页> 外文期刊>Composite Structures >GFRP hollow column to built-up beam adhesive connection: Mechanical behaviour under quasi-static, cyclic and fatigue loading
【24h】

GFRP hollow column to built-up beam adhesive connection: Mechanical behaviour under quasi-static, cyclic and fatigue loading

机译:GFRP中空柱为内置梁粘合剂连接:准静态,循环和疲劳负荷下的机械行为

获取原文
获取原文并翻译 | 示例

摘要

A new adhesive beam-column connection is tested which possess the highest strength and stiffness compared to any other similar adhesive or bolted connection tested in the past. A square GFRP hollow section, acing as a column, was connected to a built-up beam made of two GFRP U-profiles by means of either epoxy or steel bolts. The beam-column assembly formed an L-shaped frame which was tested by applying a point load at the beam free end while the column was fixed at its base. Five bolted and five adhesive replicate connections were subjected to quasi-static loading up to failure. Another three adhesive connections were subjected to 400, 800 or 1200 cycles of loading and unloading with the maximum load being equal to 0.50 P-u,P-avg, where P-u,P-avg is the average static strength of the replicate adhesive specimens. M the end of the cyclic loading, the latter specimens were loaded quasi-statically to failure. Finally, another two adhesive connections were subjected to fatigue type loading. They were successively subjected to at least 196 cycles of loading and unloading with the load amplitude being 0.50 P-u,P-avg in the first 60 cycles, 0.75 P(u,avg )in the next 60 cycles, 0.85 P-u,P-avg in the following 60 cycles and 0.95 P-u,P-avg after the 180th cycle. The test results show that the proposed adhesive connection can achieve on average 82% higher strength and 380% higher rotational stiffness than the companion bolted connection. Furthermore, the above cyclic loading has negligible effect on either the strength or the stiffness of the connection. Finally, the connection can sustain the foregoing fatigue load up to almost 180 cycles without significant damage but it will not be able to withstand the full 60 cycles of the load with 0.95 P-u,P-avg amplitude. The current results demonstrate the superior strength and stiffness of the new adhesive connection compared to a similar bolted connection.
机译:与过去测试的任何其他类似的粘合剂或螺栓连接相比,测试了一种具有最高强度和刚度的新的粘合梁柱连接。作为柱子的方形GFRP中空部分连接到由两个GFRP U形型螺栓由两个GFRP U形型制成的内置光束连接。光束柱组件形成L形框架,通过在柱固定在其基部固定时通过在无线束处施加点负荷来测试。将五个螺栓固定和五种粘合剂复制连接进行了准静态加载到失败。将另外三个粘合剂连接进行400,800或1200个循环的装载和卸载,最大载荷等于0.50p-U,P-AVG,其中P-U,P-AVG是复制粘合剂标本的平均静态强度。 M循环载荷的结束,后一种标本将准静态地装载到失败。最后,对另外两个粘合剂连接进行疲劳式载荷。它们连续地遵循至少196个装载和卸载,负载幅度为0.50 PU,P-AVG在前60个循环中的0.75 p(U,AVG),0.85 pu,p-avg在第180个循环之后以下60个循环和0.95 PU,P-AVG。测试结果表明,所提出的粘合剂连接可以平均实现82%的强度高82%,旋转刚度比伴随的螺栓连接较高380%。此外,上述循环负载对连接的强度或刚度具有可忽略的影响。最后,连接可以维持上述疲劳负载,高达180个循环,而无需显着损坏,但它将无法承受载荷的完整60周期,具有0.95p-U,P-AVG幅度。与类似的螺栓连接相比,目前的结果证明了新的粘合连接的优越强度和刚度。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号