Simultaneous Removal of Nickel and Cadmium During the Cold Purification of Zinc Sulfate Solution

机译:硫酸锌溶液的冷提纯过程中同时去除镍和镉

获取原文
获取原文并翻译 | 示例

摘要

One of the most important steps in the zinc processing industries is the removal of impurities. In this step, cobalt, nickeland cadmium are removed from the leach solution by hot and cold purification, respectively. In this research, the effectiveparameters on cold purification reactor of Dandi zinc smelting plant (Zanjan—Iran) such as temperature, consumptionof zinc dust, residence time, copper sulfate additive, pH of solution, zinc dust particle size and mixing speed are studied.Results demonstrated that optimum concentration of zinc dust to remove impurities properly is 2 g/L, which is less thanthe factory’s consumption by up to 30%. It was also found that the copper sulfate had no effect on the removal process ofnickel and cadmium, and hence exclusion of this additive can cause cost-effectiveness in the process. Optimum amounts ofresidence time, temperature, pH and mixing speed are 75 min, 80 ℃, 4.5 and 400 rpm, respectively. It was demonstratedthat the smaller particle size has more effect on the removal of nickel and cadmium. The maximum efficiency was observedat < 45 μm. More ever, the high density of zinc ions had a deterrent effect on the efficiency of nickel and cadmium removal.
机译:锌加工工业中最重要的步骤之一是去除杂质。在此步骤中,分别通过热纯化和冷纯化从浸出溶液中除去钴,镍和镉。本研究研究了丹迪锌冶炼厂(赞詹—伊朗)冷提纯反应器的有效参数,例如温度,锌粉消耗量,停留时间,硫酸铜添加剂,溶液的pH值,锌粉粒度和混合速度。表明锌粉尘的最佳去除杂质的最佳浓度为2 g / L,比工厂的消耗量少30%。还发现硫酸铜对镍和镉的去除过程没有影响,因此排除该添加剂会导致该过程的成本效益。最佳停留时间,温度,pH和混合速度分别为75分钟,80℃,4.5和400 rpm。结果表明,较小的颗粒尺寸对镍和镉的去除效果更大。在<45μm处观察到最大效率。更重要的是,高密度的锌离子对镍和镉的去除效率具有威慑作用。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号