Triangular laser-induced submicron textures for functionalising stainless steel surfaces

机译:三角激光诱导的亚微米织构,用于功能化不锈钢表面

获取原文
获取原文并翻译 | 示例

摘要

Processing technologies that engineer surfaces with sub-micron topographies are of a growing interest to a range of optical, hydrophobic and microbiological applications. One of the promising technologies for creating such topographies employs ultra-short laser pulses to produce laser-induced periodic surface structures (LIPSS) that often result in non-regular, quasi-periodic nanoripples and nanopillars. In this research near infrared ultra-short pulses of 310 fs with a circular polarisation was used to texture ferritic stainless steel workpieces. A single-step process was designed to generate low spatial frequency LIPSS (LSFL) over relatively large areas. Apart from highly regular and homogeneous parallel lines with approximately 900 nm periodicity, extraordinarily uniform triangular-LSFL in hexagonal arrangements was created. The generation of such LSFL was found to be highly repeatable but very sensitive to the used laser processing settings. Therefore, the sensitivity of triangular-LSFL formation to the used laser processing settings, i.e. pulse to pulse distance, pulse fluence and focal plane offsets, were investigated in regard to the resulting morphologies and functional properties, i.e. structural colors and super-hydrophobicity. Finally, the capability of this technology for producing uniform triangular-shaped LSFL on relatively large surface areas of stainless steel plates was studied. (C) 2018 Elsevier B.V. All rights reserved.
机译:利用亚微米形貌对表面进行工程处理的加工技术对于一系列光学,疏水和微生物学应用越来越感兴趣。创建此类地形的一项有前途的技术之一是利用超短激光脉冲产生激光诱导的周期性表面结构(LIPSS),该结构通常会导致不规则的准周期性纳米波纹和纳米柱。在这项研究中,使用具有圆极化的310 fs的近红外超短脉冲对铁素体不锈钢工件进行纹理处理。设计了一个单步过程以在相对较大的区域上生成低空间频率LIPSS(LSFL)。除了周期大约为900 nm的高度规则且均匀的平行线之外,还创建了六边形排列的非常均匀的三角形LSFL。发现这种LSFL的产生是高度可重复的,但是对所使用的激光加工设置非常敏感。因此,就所得的形态和功能特性,即结构颜色和超疏水性,研究了三角形-LSFL形成对所用激光加工设置的敏感性,即脉冲至脉冲距离,脉冲通量和焦平面偏移。最后,研究了该技术在较大的不锈钢板表面积上生产均匀的三角形LSFL的能力。 (C)2018 Elsevier B.V.保留所有权利。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号