The influence of stabilizers on the production of gold nanoparticles by direct current atmospheric pressure glow microdischarge generated in contact with liquid flowing cathode

机译:稳定剂对与液体流动阴极接触产生的直流大气压辉光微放电对金纳米颗粒生产的影响

代理获取
本网站仅为用户提供外文OA文献查询和代理获取服务,本网站没有原文。下单后我们将采用程序或人工为您竭诚获取高质量的原文,但由于OA文献来源多样且变更频繁,仍可能出现获取不到、文献不完整或与标题不符等情况,如果获取不到我们将提供退款服务。请知悉。

摘要

Gold nanoparticles (Au NPs) were prepared by direct current atmospheric pressure glow microdischarge (dc-μAPGD) generated between a miniature argon flow microjet and a flowing liquid cathode. The applied discharge system was operated in a continuous flow liquid mode. The influence of various stabilizers added to the solution of the liquid cathode, i.e., gelatin (GEL), polyvinylpyrrolidone (PVP), or polyvinyl alcohol (PVA), as well as the concentration of the Au precursor (chloroauric acid, HAuCl4) in the solution on the production growth of Au NPs was investigated. Changes in the intensity of the localized surface plasmon resonance (LSPR) band in UV/Vis absorption spectra of solutions treated by dc-μAPGD and their color were observed. The position and the intensity of the LSPR band indicated that relatively small nanoparticles were formed in solutions containing GEL as a capping agent. In these conditions, the maximum of the absorption LSPR band was at 531, 534, and 535 nm, respectively, for 50, 100, and 200 mg L−1 of Au. Additionally, scanning electron microscopy (SEM) and dynamic light scattering (DLS) were used to analyze the structure and the morphology of obtained Au NPs. The shape of Au NPs was spherical and uniform. Their mean size was ca. 27, 73, and 92 nm, while the polydispersity index was 0.296, 0.348, and 0.456 for Au present in the solution of the flowing liquid cathode at a concentration of 50, 100, and 200 mg L−1, respectively. The production rate of synthesized Au NPs depended on the precursor concentration with mean values of 2.9, 3.5, and 5.7 mg h−1, respectively.
机译:金纳米粒子(Au NPs)是通过在微型氩流微射流和流动的液体阴极之间产生的直流大气压辉光微放电(dc-μAPGD)制备的。所施加的排放系统以连续流动液体模式运行。添加到液体阴极溶液中的各种稳定剂(明胶(GEL),聚乙烯吡咯烷酮(PVP)或聚乙烯醇(PVA))的影响以及溶液中Au前体(氯金酸,HAuCl4)的浓度研究了金纳米颗粒生产增长的解决方案。在dc-μAPGD处理的溶液的UV / Vis吸收光谱中观察到了局部表面等离子体共振(LSPR)带的强度及其颜色的变化。 LSPR带的位置和强度表明,在含有GEL作为封端剂的溶液中形成了相对较小的纳米颗粒。在这些条件下,50、100和200 mg L -1 的Au的最大吸收LSPR带分别为531、534和535nm。此外,使用扫描电子显微镜(SEM)和动态光散射(DLS)来分析获得的金纳米颗粒的结构和形态。金纳米颗粒的形状为球形且均匀。他们的平均大小约为。 27、73和92nm,而流动液体阴极溶液中以50、100和200 mg L -1 。合成的金纳米颗粒的生产率取决于前体浓度,平均值分别为2.9、3.5和5.7 mg·h -1