Effects of Temperature on Bending Properties of Three-Dimensional and Five-Directional Braided Composite

机译:温度对三维五向编织复合材料弯曲性能的影响

代理获取
本网站仅为用户提供外文OA文献查询和代理获取服务,本网站没有原文。下单后我们将采用程序或人工为您竭诚获取高质量的原文,但由于OA文献来源多样且变更频繁,仍可能出现获取不到、文献不完整或与标题不符等情况,如果获取不到我们将提供退款服务。请知悉。

摘要

The bending properties of three-dimensional (3Dim) and five-directional (5Dir) braided/epoxy resin composites at room temperature, 90 °C, 110 °C, and 150 °C and heating for 0.25 h, 10 h, and 30 h, respectively, were studied. The effect of different temperatures and heating times on the bending property of these composites was discussed. The results showed that the bending strength of these composites at 90 °C, 110 °C, and 150 °C and heating time of 0.25 h is 33.86%, 46.27%, and 83.94% lower, respectively, than that at room temperature. In addition, 3Dim–5Dir braided composites exhibit different damage modes at different temperatures, revealing different failure mechanisms. Heating temperature has greater influence on the bending properties of these composites than heating time. The results provided a basis for the application of resin-based 3Dim–5Dir braided/epoxy resin composites at different temperatures.
机译:三维(3Dim)和五向(5Dir)编织/环氧树脂复合材料在室温,90°C,110°C和150°C以及加热0.25 h,10 h和30 h时的弯曲特性分别进行了研究。讨论了不同温度和加热时间对这些复合材料弯曲性能的影响。结果表明,这些复合材料在90°C,110°C和150°C的弯曲强度以及0.25 h的加热时间分别比在室温下低33.86%,46.27%和83.94%。此外,3Dim-5Dir编织复合材料在不同温度下表现出不同的破坏模式,揭示出不同的破坏机理。加热温度比加热时间对这些复合材料的弯曲性能影响更大。结果为在不同温度下应用基于树脂的3Dim-5Dir编织/环氧树脂复合材料提供了基础。