Detonation nanodiamond is a commercially available synthetic diamond that is obtained from the carbon of explosives. It is known that the average particle size of detonation nanodiamond is 4–6 nm. However, it is possible to separate smaller particles. Here we suggest a new approach for the effective separation of detonation nanodiamond particles by centrifugation of a “hydrosol/glycerol” system. The method allows for the production of the detonation nanodiamond hydrosol with a very sharp distribution in size, where more than 85% of particles have a size ranging 1–4 nm. The result is supported by transmission electron microscopy, atomic force microscopy, and dynamic light scattering.
机译:爆轰纳米金刚石是一种从炸药的碳中获得的可商购的合成金刚石。众所周知,爆轰纳米金刚石的平均粒径为4–6 nm。但是,可以分离较小的颗粒。在这里,我们提出了一种通过离心“水溶胶/甘油”系统有效分离爆轰纳米金刚石颗粒的新方法。该方法可以生产尺寸非常尖锐的爆轰纳米金刚石水溶胶,其中超过85%的颗粒的尺寸范围为1-4 nm。该结果得到透射电子显微镜,原子力显微镜和动态光散射的支持。