A method for increasing the size of nanocrystals detonation nanodiamond, comprising annealing by heating to a high temperature a mixture consisting of powder detonation nanodiamond and intermetallic compounds, characterized in that a powder mixture of 50% (wt.) Mixture containing 90% (wt.) detonation nanodiamond powder and 10% (wt.) of aluminum powder, and 50% (wt.) mixture of intermetallic nickel and aluminum, the appropriate stoichiometric NiAl or NiAl, then the mixture was mixed thoroughly and compressed to form cylinders, samples annealed in vacuo at a pressure no worse than 10 mm at a temperature of 950 ° C for 30 minutes.
机译:一种增加纳米晶体爆轰纳米金刚石尺寸的方法,其包括通过将由粉末爆轰纳米金刚石和金属间化合物组成的混合物加热至高温进行退火,其特征在于50%(wt。)混合物的粉末混合物包含90%(wt。%)的粉末。 )爆轰纳米金刚石粉和10%(wt。)的铝粉,以及50%(wt。)的金属间镍和铝的混合物,适当的化学计量的NiAl或NiAl,然后将混合物充分混合并压缩以形成圆柱体,并进行退火在真空中,在不低于10 mm的压力下,在950°C的温度下保持30分钟。

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号