In the ore dressing tests of a scheelite deposit from Hunan Province, technical parameters for pulp conditioning and hydrophobic aggregation were optimized, through which the apparent diameter of scheelite was regulated, and a scheelite bulk concentrate with WO3 grade and recovery of 10. 44% and 86. 72%, respectively, was collected. Compared with the conventional flotation, the scheelite roughing recovery can be up 2. 09 percentage point, while the recovery for fine⁃grained (-10 μm) scheelite can be raised from 64.74% to 75.88%.%对湖南某白钨矿开展了选矿试验研究,通过强化调浆⁃疏水聚团工艺,调整白钨矿表观粒径,可获得品位10.44%、回收率86.72%的白钨粗精矿。相比常规浮选,白钨粗选段选矿回收率提高了2.09个百分点;微细粒级(-10μm)白钨矿回收率由64.74%提高至75.88%。