摘要

There is 3. 60% lead and 9. 19% zinc in a lead-zinc oxide ore from Sichuan. The oxide rate of lead and zinc is above 90%. It is fine-grained dissemination,being a refractory lead-zinc ore. Experimental study was conducted to provide technique basis for the exploitation and utilization of the ore. Results show that at the grinding fineness of 96. 74% passing 325 mesh ,lead concentrate with lead grade of 48. 61%,recovery of 86. 15%,zinc concentrate with zinc grade of 40. 14%,recovery of 65. 04% was obtained by the process of one-roughing,three-cleaning,one-scavenging using Na2 S as regulator,amyl-xanthate as lead collector to preferential floating lead, and lead flotation tailings via the process of one-roughing, three-cleaning, two-scavenging with Na2 S as sulfurizing reagent,AgNO3 as activator,sodium silicate as dispersants and inhibitors for gangue miner-als ,octadecylamine as collector to select zinc.%四川某氧化铅锌矿石铅、锌品位分别为3.60%和9.19%,矿石氧化程度非常高,铅、锌氧化率高达90%左右,且主要铅、锌矿物嵌布粒度微细,属难选铅锌矿石.为确定该矿石的合理选矿工艺,对矿石进行了选矿试验.结果表明,在磨矿细度为-325目占96.74%情况下,以硫化钠为铅矿物硫化剂、戊基黄药为浮铅捕收剂,以硫化钠为锌矿物硫化剂、硝酸银为活化剂、水玻璃为矿泥分散剂和脉石矿物抑制剂、十八胺为浮锌捕收剂,采用1粗1扫3精选铅、1粗2扫3精选锌、中矿闭路返回流程处理该矿石,可获得铅品位为48.61%、回收率为86.15%的铅精矿,锌品位为40.14%、回收率为65.04%的锌精矿.

著录项

  • 来源
    《金属矿山》 |2016年第11期|85-88|共4页
  • 作者单位

    武汉理工大学资源与环境学院,湖北 武汉430070;

    武汉理工大学资源与环境学院,湖北 武汉430070;

    武汉理工大学资源与环境学院,湖北 武汉430070;

    武汉理工大学资源与环境学院,湖北 武汉430070;

  • 原文格式 PDF
  • 正文语种 chi
  • 中图分类 TD923+.7;
  • 关键词

    氧化铅锌矿; 浮选; 活化剂;

相似文献

  • 中文文献
  • 外文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号