Experimental Research on the Pellets of Brazilian Iron Concentrate

机译:巴西铁精矿球团试验研究

获取原文

摘要

In this paper, the method of preparing green balls from Brazilian iron concentrate was studied. The hematite and two kinds of magnetite concentrate were the main raw materials, the effects of the dosage of bentonite, pelletizing moisture, pelletizing time, particle size, and the ratio of the two magnetite concentrates on the green balls' strength were studied. When using 1.0-1.3% Indian bentonite, the pelletizing moisture of 9.5-10%, the pelletizing time of 12-15 min, the mineral powder particle size under the condition of -325 mesh 85-90%, it is suitable for pelletizing. And the falling strength of the green balls is 3.0 times 0.5 m~(-1), the compressive strength is 16-23 N/P, the decrepitation temperature of the green balls is above 350 °C. After blending with the magnetic concentrate, the decrepitation temperature of the green balls rises, but the strength decreases, and the amount of bentonite needs to be increased.
机译:本文研究了用巴西铁精矿制备生球的方法。以赤铁矿和两种磁铁矿精矿为主要原料,研究了膨润土用量、造球水分、造球时间、粒度以及两种磁铁矿精矿的配比对生球强度的影响。当使用1.0-1.3%的印度膨润土,造粒水分9.5-10%,造粒时间12-15min,矿粉粒度在-325目85-90%的条件下,适合造粒。生球的坠落强度为0.5m-1的3.0倍,抗压强度为16-23N/P,生球的爆裂温度在350℃以上。与磁精矿混合后,生球的爆裂温度升高,但强度降低,需要增加膨润土的用量。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号